MWCNT Aqueous Conductive Slurry XN-SN375
SKU: XN-SN375
MWCNT Aqueous Conductive Slurry XN-SN375 is a black, water-based multi-walled carbon nanotube conductive slurry with an 18–50 nm outside diameter, 5.0 ± 0.25 wt% solids, and ≤10,000 mPa·s viscosity for lithium-ion battery electrodes and conductive composite applications.
Need a bulk order or custom specification? Request a competitive quote today!
Name: MWCNT Aqueous Conductive Slurry
Material Type: Water-Based Multi-Walled Carbon Nanotube Conductive Slurry
Product Code: XN-SN375
Brand: Xnergy
Product Introduction:
XN-SN375 is a water-based conductive slurry containing multi-walled carbon nanotubes with an outside diameter of 18–50 nm and a length of ≤20 μm. The 5.0 ± 0.25 wt% solid content and controlled dispersion provide a practical conductive additive for lithium-ion battery electrode formulations and other conductive composite systems.
Key Features:
High-aspect-ratio MWCNT conductive network
Water-based slurry format
18–50 nm nanotube outside diameter
5.0 ± 0.25 wt% controlled solid content
≤10,000 mPa·s viscosity
High electrical and thermal conductivity potential
Large specific surface area
Suitable for battery electrodes and conductive composites
Technical Specifications:
| Parameter | Specification |
|---|---|
| Material | Multi-walled carbon nanotube (MWCNT) aqueous conductive slurry |
| Appearance | Black paste |
| MWCNT Outside Diameter | 18–50 nm |
| MWCNT Length | ≤20 μm |
| Solid Content | 5.0 ± 0.25 wt% |
| Carbon Content | 4.0 ± 0.15 wt% |
| Dispersant Content | 1.0 ± 0.2 wt% |
| Viscosity | ≤10,000 mPa·s |
| Reference Addition for LFP Systems | Approximately 1–2%; optimize for the formulation |
| Storage | 5–35 °C; relative humidity below 80%; protect from direct sunlight |
| Unopened Shelf Life | 6 months under the specified storage conditions |
Application Areas:
LFP lithium-ion battery electrode formulations
Lithium-ion battery anode formulations
Conductive polymer and nanotube composites
Supercapacitors and energy-conversion materials
Sensors, catalysts, field emitters, and composite reinforcement
Storage Conditions:
Store at 5–35 °C and relative humidity below 80%, away from direct sunlight. The unopened shelf life is 6 months under the specified conditions. A viscosity change during long-term room-temperature storage can occur and should be considered during formulation preparation.
Note: Published specifications are based on single measurements; minor batch-to-batch variation may occur. Verify the addition level and processing conditions for the target formulation. Related products: XN-SWCNT-01SH Water-Based SWCNT Slurry for Lithium Battery Applications (Black Liquid), XN-CNT-HC801SN Water-Based MWCNT Conductive Slurry for Battery Applications (Black Liquid), Carbon nanotube conductive slurry, Carbon black C02 for Batteries.