NCM811 Cathode Disc (Ø15 mm) for Coin Cell | Single-Sided Coated
SKU: XN-NCM811-D15
Free Shipping$270.00
NCM811 Cathode Disc (Ø15 mm, Single-Sided) — NCM811 (Ni 80%, Co 10%, Mn 10%) on 16 μm Al foil; coating 10.5 ± 0.20 mg/cm², compacted density 2.75 ± 0.1 g/cm³; AM content 95%; 100 sheets/box.
Reference capacity 190 mAh/g at 0.1C (3.0–4.3 V). Designed for CR2032 coin cell assembly.
Need a bulk order? Request a competitive quote today!
Name: NCM811 Cathode Disc (Ø15 mm) for Coin Cell | Single-Sided Coated
Material Type: NCM811 (Ni 80%, Co 10%, Mn 10%) on 16 μm Aluminum Foil, Ø15 mm Disc
Product Code: XN-NCM811-D15
Product Introduction:
NCM811 is a high-nickel lithium nickel cobalt manganese oxide cathode (Ni 80%, Co 10%, Mn 10%). This Ø15 mm single-sided cathode disc is coated on 16 μm aluminum foil and specifically designed for lithium-ion coin cell assembly and laboratory-scale battery research. Coating areal density is 10.5 ± 0.20 mg/cm², compacted density 2.75 ± 0.1 g/cm³, and reference specific capacity is 190 mAh/g at 0.1C (3.0–4.3 V). Supplied 100 sheets/box.
Key Features:
NCM811 (Ni 80%, Co 10%, Mn 10%) — high-nickel cathode for high energy density
Ø15 mm single-sided disc for CR2032 coin cell assembly
Coating areal density 10.5 ± 0.20 mg/cm²
Compacted density 2.75 ± 0.1 g/cm³
Reference specific capacity 190 mAh/g at 0.1C (3.0–4.3 V)
Current collector: 16 μm aluminum foil, 4.22 mg/cm²
Active material weight ratio 95%
Packaging: 100 sheets/box
Specifications:
| Parameter | Specification |
|---|---|
| Electrode Size | Ø15 mm |
| Coating Type | Single-sided coating (calendered) |
| Current Collector Thickness (μm) | 16 |
| Coating Areal Density (mg/cm²) | 10.5 ± 0.20 |
| Compaction Density (g/cm³) | 2.75 ± 0.1 |
| Current Collector Areal Density (mg/cm²) | 4.22 |
| Active Material Weight Ratio | 95% |
| Voltage Range | 3.0–4.3 V |
| Reference Specific Capacity | 190 mAh/g (0.1C) |
| Packaging | 100 sheets/box |
Storage & Handling:
After opening, please keep the electrode disc sealed and store in a glove box or in a drying oven at 60°C.
Note: Specifications are for reference only. Actual electrochemical performance depends on counter/reference electrode selection, electrolyte, separator, cell assembly conditions, and cycling protocol. For anode electrode sheets, see the Anode Materials category. For electrolytes, see the Electrolytes category. For coin cell assembly components, see Coin Cells & Hardware.