SWCNT Aqueous Conductive Slurry XN-SN377
SKU: XN-SN377
SWCNT Aqueous Conductive Slurry XN-SN377 is a black, water-based single-walled carbon nanotube conductive slurry with a 1–2 nm outside diameter, 1.0 ± 0.03 wt% solids, and ≤5,000 mPa·s viscosity for silicon–carbon anodes and advanced conductive composite applications.
Need a bulk order or custom specification? Request a competitive quote today!
Name: SWCNT Aqueous Conductive Slurry
Material Type: Water-Based Single-Walled Carbon Nanotube Conductive Slurry
Product Code: XN-SN377
Brand: Xnergy
Product Introduction:
XN-SN377 is a water-based conductive slurry containing single-walled carbon nanotubes with a 1–2 nm outside diameter and a length of ≤50 μm. Its high-aspect-ratio SWCNT network, 1.0 ± 0.03 wt% solid content, and controlled dispersion support low-addition conductive pathways in silicon–carbon anodes and other advanced electrode formulations.
Key Features:
1–2 nm single-walled carbon nanotube structure
High-aspect-ratio conductive network at low addition levels
Water-based slurry format
1.0 ± 0.03 wt% controlled solid content
≤5,000 mPa·s viscosity
≤150 ppb magnetizable metal content
High electrical and thermal conductivity potential
Large specific surface area
Technical Specifications:
| Parameter | Specification |
|---|---|
| Material | Single-walled carbon nanotube (SWCNT) aqueous conductive slurry |
| Appearance | Black paste |
| SWCNT Outside Diameter | 1–2 nm |
| SWCNT Length | ≤50 μm |
| Solid Content | 1.0 ± 0.03 wt% |
| Carbon Content | 0.4 ± 0.03 wt% |
| Dispersant Content | 0.6 ± 0.03 wt% |
| Viscosity | ≤5,000 mPa·s |
| Magnetizable Metal | ≤150 ppb |
| Reference Addition for Silicon–Carbon Anodes | Approximately 0.01–0.08%; optimize for the formulation |
| Storage | 5–35 °C; relative humidity below 80%; protect from direct sunlight |
| Unopened Shelf Life | 6 months under the specified storage conditions |
Application Areas:
Silicon–carbon lithium-ion battery anodes
EV, high-capacity aluminum-can, pouch, and polymer lithium-ion batteries
Conductive polymer and nanotube composites
Supercapacitors and energy-conversion materials
Sensors, catalysts, field emitters, and composite reinforcement
Storage Conditions:
Store at 5–35 °C and relative humidity below 80%, away from direct sunlight. The unopened shelf life is 6 months under the specified conditions. A viscosity change during long-term room-temperature storage can occur and should be considered during formulation preparation.
Note: Published specifications are based on single measurements; minor batch-to-batch variation may occur. Verify the addition level and processing conditions for the target formulation. Related products: MWCNT Aqueous Conductive Slurry XN-SN375, XN-SWCNT-01SH Water-Based SWCNT Slurry for Lithium Battery Applications (Black Liquid), XN-CNT-HC801SN Water-Based MWCNT Conductive Slurry for Battery Applications (Black Liquid), Carbon nanotube conductive slurry.